牌號(hào)
|
SUH660耐熱鋼棒和線材
|
|
|
|
|
|
|
|
|
|
|
|
|
對(duì)應(yīng)標(biāo)準(zhǔn)
|
JIS G 4311-2019
|
|
|
|
|
|
|
|
|
|
|
|
|
耐熱鋼棒和線材
|
|
|
|
|
|
|
|
|
|
|
|
|
Heat-resisting steel bars and wire rods
|
|
|
|
|
|
|
|
|
|
|
|
|
歸類
|
奧氏體不銹鋼
|
|
|
|
|
|
|
|
|
|
|
|
|
性能
|
耐腐蝕
|
|
|
|
|
|
|
|
|
|
|
|
|
標(biāo)簽
|
耐熱鋼棒 鐵鉻鎳高溫合金
|
|
|
|
|
|
|
|
|
|
|
|
|
說(shuō)明
|
①本標(biāo)準(zhǔn)適用于耐熱鋼棒(圓鋼、角鋼、六角鋼及扁鋼的統(tǒng)稱,稱為棒材)及耐熱鋼線材(稱為線材)。
|
|
|
|
|
|
|
|
|
|
|
|
|
②牌號(hào)后綴“-B”(熱軋棒材);后綴“-CB”(冷軋棒材)
|
|
|
|
|
|
|
|
|
|
|
|
|
例如:熱軋棒材SUH1-B,SUS304-HR-B
|
|
|
|
|
|
|
|
|
|
|
|
|
冷軋棒材SUH1-CB,SUS304-HR-CB
|
|
|
|
|
|
|
|
|
|
|
|
|
③牌號(hào)后綴“-WR”表示線材。例如:SUH1-WR,SUS304-HR-WR
|
|
|
|
|
|
|
|
|
|
|
|
|
SUH660 化學(xué)元素成分含量(%)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
成分
|
C
|
Si
|
Mn
|
P
|
S
|
Cr
|
Ni
|
Mo
|
Ti
|
V
|
B
|
Al
|
|
最小值
|
-
|
-
|
-
|
-
|
-
|
13.5
|
24
|
1
|
1.9
|
0.1
|
0.001
|
-
|
|
最DA值
|
0.08
|
1
|
2
|
0.04
|
0.03
|
16
|
27
|
1.5
|
2.35
|
0.5
|
0.01
|
0.35
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
SUH660 機(jī)械性能
|
|
|
|
|
|
|
|
|
|
|
|
|
|
條件
|
熱處理或狀態(tài)
|
抗拉強(qiáng)度
|
屈服點(diǎn)
|
延伸率
|
斷面收縮率
|
硬度
|
|
|
|
|
|
|
|
σb
|
σs
|
δ
|
ψ
|
HBW
|
|
|
|
|
|
|
|
Mpa
|
Mpa
|
%
|
%
|
|
|
|
|
|
|
|
|
棒材;d≤180
|
固溶處理+時(shí)效 (H)
|
≥900
|
≥590
|
≥15
|
≥18
|
≥248
|
|
|
|
|
|
|
|
熱處理?xiàng)l件:固溶處理 溫度885~915°C,快冷或965~995°C,快冷;時(shí)效處理 700~760°C保持16h,空冷或緩慢冷卻
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|